T.C. 745 |
DESCRIPTION
T.C. 745 is a carefully blended liquid acid material designed for use in the final rinse
solution of 3 or 5 stage iron phosphating installations. This product is orange in color, stable and readily
miscible with water at use dilutions. The use of T.C. 745 is recommended to enhance the corrosion resistance
of iron phosphate coatings and to generally condition the surface prior to subsequent finishing.
OPERATION
T.C. 745 may be used at a concentration of 1/4 to 1 pint per 100 gallons of solution, in a
temperature range of room temperature to 130°F. Exposure time is 30 seconds. Adjust these operating conditions
as required for optimum results.
SAFETY PRECAUTIONS
The usual precautions for handling acid materials are to be observed. Avoid skin and eye
exposure. In case of accident, flush affected areas with copious quantities of water and get medical attention.
Working personnel handling T.C. 745 solution should wear rubber gloves, goggles and other proper protective
clothing. Do not allow dehydrating in presence of paper or cloth.
DO NOT TAKE INTERNALLY.
9/2000
|